Anatomical Injections

1. Tallow, resin, and wax, equal parts; melt over a slow fire; and add red lead or vermilion sufficient to colour. For coarse preparations.

2. A strong solution of isinglass, coloured as required. For delicate preparations.

3. Amalgam Injection. Melt together 1 oz. each of bismuth, lead, and zinc, and, when melted, add 2 oz. of quicksilver. Also for delicate parts.

Parisian Bronzing Pastes

1. Plumbago 1 oz., sienna

2 oz., rouge 1/2 oz. Add a few drops of hydrosulphate of ammonia, and water.

2. Chrome lead 2 oz., Prussian blue 2 oz., plumbago 1/2 lb., sienna powder and lake carmine, each 1/4 lb. Add sufficient water to make a paste. Brosse de Coeail. The roots of lucerne (Medicago sativa), cleaned, dried, and hammered at the end. Used as a tooth-brush.