How To Bleach Ivory

Take a double handful of lime, and slake it by sprinkling it with water; then add three pints of water, and stir the whole together; let it settle ten minutes, and pour the water into a pan. Take the ivory, and steep it in the lime-water for twenty-four hours, after which boil it in a strong alum-water one hour, and dry it in the air.

Artificial Ivory

Two parts of caoutchouc are dissolved in 36 parts of chloroform, and the solution is saturated with pure gaseous ammonia. The chloroform is then distilled off at a temperature of 850 C. (1850 F.) The residue is mixed with calcium phosphate or zinc carbonate, pressed into moulds and dried.

When calcium phosphate is used, the product possesses to a considerable degree the nature and composition of ivory.

Cement For Joining Leather

A cement which has been found useful for this purpose may be prepared by mixing ten parts of bisulphate of carbon, one of oil of turpentine, and so much gutta-percha as is necessary to produce a thick fluidity. The leather must be first freed from all grease, which can be done by simply laying it in a cloth and pressing this with a hot iron. The parts to be joined, after being brought into contact with the cement, require to be kept pressed together until they are quite dry.

Cement For Leather And Wood

Equal parts of pitch and gutta-percha melted together. This compound is insoluble in water.

Cement For Joining China, Etc

Beat the whites of eggs well to a froth, let them settle, add soft grated or sliced cheese and quicklime; beat them well together, and apply a little to the broken edges. This cement will endure both fire and water.

Cement For China, Etc

Pound half an ounce of resin and four ounces of gum-mastic; put them into a pipkin on the fire to melt; stir them well. To this add about half an ounce of finely-powdered glass, and half an ounce of quicklime; stir the whole well together. When nearly cold, form it into sticks, on a stone, in the same manner as sticks of sealing-wax are formed. When it is desired to cement any article, heat the broken edges sufficiently to melt the cement, which rub thinly on both edges; bring them accurately together; press them close, and let them cool. If this be carefully done, the work will sooner break in any other part than where the cement has been applied.

Cement For Glass

Steep one ounce of isinglass in half a pint of spirits of wine for twenty-four hours; then let it dissolve over a slow fire (always keeping it covered, or the spirit will evaporate); now well bruise six cloves of garlic in a mortar, put them in a linen cloth, and squeeze the juice into the isinglass; mix all well together, and keep it for use. It is excellent to join glass ornaments, etc.

Cements For Aquariums

Take 1 gill of plaster-of-Paris, 1 gill of litharge, 1 gill of fine white sand, 1/2 gill of finely-powdered resin. Mix well, and bottle and cork it until wanted for use, then mix it with boiled oil and dryers until as thick as putty. Mix the cement only in small quantities as it dries quickly.

Mix boiled linseed oil, litharge, red and white lead together, using white lead in the largest proportion, spread on flannel, and place on the joints.

A solution of glue, 8 oz. to 1 oz. of Venice turpentine; boil together, agitating all the time, until the mixture becomes as complete as possible, the joints to be cemented to be kept together for forty-eight hours if required.

Take 1/2 a gill of gold size, 2 gills of red lead, 1 1/2 gill of litharge, and sufficient silver-sand to make it into a thick paste for use. This mixture sets in about two days.