This section is from the book "Hints And Practical Information For Cabinet-Makers, Upholsterers, And Furniture Men Generally", by John Phin. Also available from Amazon: Hints And Practical Information For Cabinet-Makers, Upholsterers, And Furniture Men.
Lacquers are frequently required to be colored, either of yellow or red tints. For yellow tints, turmeric, cape aloes, saffron, or gamboge are employed; and for red tints, annotto and dragon's-blood are used-the proportions being varied according to the color required. Thus, for a pale yellow, about one ounce of gamboge and two ounces of cape aloes are powdered and mixed with one pound of shell-lac. For a full yellow, half a pound of turmeric and two ounces of gamboge, and for a red lacquer, half a pound of dragon's-blood and one pound of annotto. The color is also modified by that of the lac employed, the best pale or orange shell-lac being used for light-colored lacquers, and dark-colored shell-lac or seed-lac is used for the darker tints. For pale lacquers, sandarac is sometimes used with the shell-lac. Thus a pale gold-colored lacquer is made with eight ounces of shell-lac, two ounces of sandarac, eight ounces of turmeric, two ounces of annotto, and a quarter of an ounce of dragon's-blood to one gallon of spirit of wine.
The most convenient method, however, of coloring lacquers, is to make a saturated solution in spirit of wine of each of the coloring matters, and to add the solutions in different proportion to the pale lacquer according to the tint required; but the whole of the coloring matters are not generally used by the same makers, and solutions of turmeric, gamboge and dragon's-blood afford sufficient choice for ordinary purposes. The turmeric gives a greenish-yellow tint, and, with the addition of a little gamboge, is the coloring matter employed in making the so-called green lacquer used for bronzed works.
Another mode of making lacquer: Four ounces of shell-lac and a quarter of an ounce of gamboge are dissolved by agitation, without heat, in twenty-five ounces of pure pyro-acetic ether. The solution is allowed to stand until the gummy matters not taken up by the spirit subside; the clear liquor is then decanted, and when required for use is mixed with eight times its quantity of spirit of wine. In this case, the pyro-acetic ether is employed for dissolving the shell-lac in order to prevent any but the purely resinous portions being taken up, which is almost certain to occur with ordinary spirit of wine, owing to the presence of water; but if the lacquer were made entirely with pyro-acetic ether, the latter would evaporate too rapidly to allow time for it to be equally applied.
Mastic Varnish, for painting, and similar purposes, is sometimes made in small quantities with spirit of wine; but, more generally, oil of turpentine is employed as the solvent, the proportion being about three pounds of mastic to the gallon of turpentine. For the best varnish, the mastic is carefully picked and dissolved by agitation without heat, exactly as for the best white hard varnish; after the mastic varnish has been strained it is poured into a bottle, which is loosely corked and exposed to the sun and air for a few weeks; this causes a precipitation, from which the clear varnish may be poured off for use; but the longer the varnish is kept the better it becomes.
Mastic varnish works very freely, but it is liable to chill, and the surface frequently remains tacky for some time after the varnish is applied. To prevent the latter evil, it is recommended, before dissolving the mastic, to bruise it slightly with a muller, and pick out all the pieces that are too soft to break readily, and which may be used for common varnish. To prevent the chilling, which arises from the presence of moisture, Mr. W. Neil recommends a quart of river sand to be boiled with two ounces of pearl-ash; the sand is afterwards to be washed three or four times with hot water, and strained each time. The sand is then to be dried in an oven, and when it is of a good heat, half a pint of the hot sand is to be poured into each gallon of varnish, and shaken well for five minutes; it is then allowed to settle, and carries down the moisture of the gum and turpentine.
In making common varnish, heat is generally employed to dissolve the mastic, and about one pint of turpentine varnish is added to every gallon of varnish.
 
Continue to: